To eliminate shrinkage porosity and hot tearing in cast aluminum (such as A356-T6 or A380), maintain uniform wall thickness (2.5–4.0 mm for gravity/low-pressure casting; 1.5–3.0 mm for high-pressure die casting), limit adjacent thickness ratios to ≤ 1.5:1 using gradual tapers (3:1 to 4:1 length-to-step ratio), set internal fillet radii to 0.5×–1.0× the thinner wall thickness (minimum 2.0–3.0 mm), and apply 1°–2° external draft angles (2°–4° on internal cores).
Thermodynamic & DFM Engineering Standards:
Aluminum alloys exhibit high thermal conductivity and a wide freezing range (especially Al-Si-Cu and Al-Si-Mg families), making abrupt geometric transitions prone to isolated liquid pockets and solidification cracking:
Fillet Radii & Hot-Spot Prevention:
Internal Fillets: Sharp 90° internal corners create localized heat concentration ("hot spots") in the mold, causing the junction to solidify last and form micro-shrinkage cavities. Sizing internal fillets at 0.5× to 1.0× wall thickness (e.g., a 2.5 mm fillet on a 4.0 mm wall) reduces stress concentration by up to 85%–90% and promotes smooth directional feeding toward risers.
Outer Radii: Design outer corner radii using the formula=Rinner+T (wall thickness) to preserve constant cross-sectional thickness around bends.
Thick-to-Thin Wall Transitions:
When a mounting boss or flange must be thicker than the adjoining web, avoid abrupt steps. Transition over a slope length at least 3 to 4 times the thickness difference, or core out heavy bosses to keep wall sections within ±25% of the nominal wall thickness.
Process-Specific Draft Angles:
Gravity Die Casting (Permanent Mold) & Sand Casting: Specify 1.5°–2.5° on exterior walls and 2.5°–4.0° on internal pockets or sand cores to prevent drag marks during ejection.
High-Pressure Die Casting (HPDC): Because aluminum shrinks tightly onto steel cores during rapid cooling, external walls require 0.5°–1.5° draft while internal ribs and cored holes require 1.5°–3.0° (with 3°–5° recommended for deep, narrow pockets in A380/ADC12).
Quality Impact:
Validating wall transitions and fillet geometry via solidification simulation (such as MAGMAsoft) prior to cutting steel tooling routinely lowers internal X-ray porosity scrap rates from the industry average of 4%–7% down to under 1.2%, preventing costly vacuum impregnation on pressure-tight housings.